I'm sure that this is an easy question for most, but I am wondering how an internal spline is cut. For that matter, how is an external spline cut.
 
Replies continue below

Recommended for you

Internal splines are often broached. They could be cut in a shaping machine at a pinch. The world's your lobster for external splines- they could be rolled, cut in a shaper machine, milled, or I suppose even carved out with a chisel. Basically any way you can make a gear.