I can't seem to figure out where occasional slag is coming from. I am continuously welding 321 S/S tube at 40ipm, 50-55amps, and using helium and argon for shielding gas. The slag only appears every 20-40 feet, is sometimes 3-5 droplets or a short soid layer. I am asuming it is contamination of some type but can't find what is causing it. Also, this condition does not exist at 30ipm and 40 amps. Any ideas would be helpful.