-SA-320, B8, Cl1 bolt material is classified as low strength in ASME B16.5.
-ASME B16.5 limits low strength bolting to 300# ratings or less.
-SA-320, B8, Cl2 bolting is classified as intermediate strength per ASME B16.5 and can be used in any flange rating (with qualifications on verifying the integrity).
The problem is that the allowable stress for Cl2 bolting above 1.25" diameter is the same as Cl1 bolting per II-D. I need stronger bolts for a 900# flange (1.375" diameter bolts) at a temperature of -270°F. Both SA-320 B8, Cl1 & Cl2 are OK at this temperature, but in the larger sizes the Cl2 offers no apparent benefit.
Is anyone familiar with another low temperature bolting material, acceptable by ASME VIII-1 that has higher strength than B8, Cl1?
Thanks in advance for the assistance.
-ASME B16.5 limits low strength bolting to 300# ratings or less.
-SA-320, B8, Cl2 bolting is classified as intermediate strength per ASME B16.5 and can be used in any flange rating (with qualifications on verifying the integrity).
The problem is that the allowable stress for Cl2 bolting above 1.25" diameter is the same as Cl1 bolting per II-D. I need stronger bolts for a 900# flange (1.375" diameter bolts) at a temperature of -270°F. Both SA-320 B8, Cl1 & Cl2 are OK at this temperature, but in the larger sizes the Cl2 offers no apparent benefit.
Is anyone familiar with another low temperature bolting material, acceptable by ASME VIII-1 that has higher strength than B8, Cl1?
Thanks in advance for the assistance.