hector002
Mechanical
- Jan 11, 2006
- 20
I have a block of low carbon steel with a 3.543 (90mm) bore located to within half a tenth. Does anyone know of or have a source/rule of thumb that would allow me to find a maximum tempurature i could heat the block up to before I have to start worrying about the relaxation/release of internal stresses that could shrift the alignment/roundness of my bore.