Òur steam inlet strainer to a siemans HP (100 bar) Turbine has deteriorated on repeated occasions such that the strainer elements found their way to the turbine nozzle block and became trapped there. Can anyone explain why this is occuring? We have almost eliminated the strainer as being a design flaw as it is wotking good on two other similar plants. The only difference in the piping run, however, is that this plant has a 400mm to 200mm reducer immediately before the strainer while the other plants have a 300mm to 200mm reducer.