Hello,
I am relatively new to injection molding and have been greeted with an issue regarding two lines that appear as cracks radiating out from holes molded into our facia panels where we mount switches. They appear to be where the plastic flows around the mounting hold feature in the mold and meet plastic from the other side. It does not appear to adversly affect the strength of the part but is still not desirable.
Do you have any suggestions on cause/corrective action? Thank you in advance for your assistance.
I am relatively new to injection molding and have been greeted with an issue regarding two lines that appear as cracks radiating out from holes molded into our facia panels where we mount switches. They appear to be where the plastic flows around the mounting hold feature in the mold and meet plastic from the other side. It does not appear to adversly affect the strength of the part but is still not desirable.
Do you have any suggestions on cause/corrective action? Thank you in advance for your assistance.