Mar 10, 2010 #1 Dancalifornia Mechanical Joined Mar 10, 2010 Messages 1 Location US Does anyone know what the Yick Sang equivalent texture is for Mold-Tech 11020 texture? Thanks.
Mar 10, 2010 #2 loughnane Mechanical Joined Jan 3, 2010 Messages 108 Location US Quick searched popped up this gem over @ finishing.com... Yick Sang YS 1287 appears closest to Mold-Tech MT-11020 Both textures are .0015" deep (.040 mm) Both textures specify 2.5 degrees minimum draft. Chris Loughnane - Product Design http://www.pdnotebook.comhttp://www.twitter.com/DesignNotebook Upvote 0 Downvote