Mar 18, 2005 #1 gearman1234 Mechanical Joined Dec 3, 2002 Messages 104 Location CA Does any body has any information about KROMITE # 3 composition and mechanical properties?
Mar 18, 2005 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US Here is the information you require. I might add that keep this material in our shop for routine use. Look at the 2nd PDF http://www.associatedsteel.com/products-steelbars.shtml Upvote 0 Downvote
Here is the information you require. I might add that keep this material in our shop for routine use. Look at the 2nd PDF http://www.associatedsteel.com/products-steelbars.shtml
Mar 18, 2005 Thread starter #3 gearman1234 Mechanical Joined Dec 3, 2002 Messages 104 Location CA Thanks for the info. But there is no chemical composition specified. I wanted to check if that is close to 4140/4340 or similar steel. Upvote 0 Downvote
Thanks for the info. But there is no chemical composition specified. I wanted to check if that is close to 4140/4340 or similar steel.
Mar 18, 2005 #4 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US It is close, if you give them a call they will fax you the information. We essentially use it for 4140 HT in our machine shop. I may still have a hard copy of their catalogue I’ll try to locate it as it has the compositions of all their products. Upvote 0 Downvote
It is close, if you give them a call they will fax you the information. We essentially use it for 4140 HT in our machine shop. I may still have a hard copy of their catalogue I’ll try to locate it as it has the compositions of all their products.
Mar 24, 2005 Thread starter #5 gearman1234 Mechanical Joined Dec 3, 2002 Messages 104 Location CA Thanks for the info Upvote 0 Downvote