Does any body has any information about KROMITE # 3 composition and mechanical properties?
 
Replies continue below

Recommended for you

Thanks for the info. But there is no chemical composition specified. I wanted to check if that is close to 4140/4340 or similar steel.
 
It is close, if you give them a call they will fax you the information.
We essentially use it for 4140 HT in our machine shop.

I may still have a hard copy of their catalogue I’ll try to locate it as it has the compositions of all their products.
 