Hi,
I'm searching information about the steel 27MnVs6, mechanical characteristics and applications. Can anybody help me, please?.

Emiaj
 
The correct designation for this grade is 27MnSiVS6. The DIN Werkstoff Nummer is 1.5232. It was developed as a ferritc-pearlitic steel for precipitation hardening from hot-working temperatures. It has been replaced by the new grade 30MnVS6 (1.1302) in DIN EN 10267. There are a couple of links below for papers written on the old grade:



Perform a google search using 30MnVS6 and/or DIN 10267 to find additional information.
 
Hi TVP,
Thank you very much for the information, it has been very valuable for me.

Bye