I am trying to find the construction material: steel anchor bolt to concrete, concrete anchor bolt adhesive, combustion temperature and found no information.

-I know a guy what coated his job site tool box in expired anchor bolt adhesive on the inside and it was almost impossible to grind through he said.

-what is the best grout/steel apoxy to use for this application?

-Diamond dust could also be applied with the adhesive or put into the material.

If you could imagine the marketability of a impenetrable toolbox and make a patent I would buy one.

(Currently what is the best material I could use to mix with diamond powder with a high flash point with some elasticity) like Hilti hy-150
 
Spray on truck bed liner has been tested for making cement walls blast proof if I recall correctly.
Also, I believe that most anchor bolt grout is an epoxy base.
 
The title of this thread sorta reminded me of this cartoon...

Nonsequitur71033_CEO-Engr_Jobs_keisxp.gif


Regards, Wil Taylor
o Trust - But Verify!
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation, Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", HBA forum]
o Only fools and charlatans know everything and understand everything." -Anton Chekhov
 
-I know a guy what coated his job site tool box in expired anchor bolt adhesive on the inside and it was almost impossible to grind through he said.

Apocryphal, at best; angle grinders can grind through steel, hard to imagine not being able to grind through epoxy.

-Diamond dust could also be applied with the adhesive or put into the material

Diamond dust, or other hard dusts, are used to make grinder wheels, and they're a high proportion of the wheel material. This means that you would need a comparable proportion in your adhesive, which would make it a poor adhesive and quite expensive. Imagine covering your toolbox with grinder wheels.

By the way, it took all of 5 seconds to find this with your text

TTFN (ta ta for now)
I can do absolutely anything. I'm an expert! faq731-376 forum1529 Entire Forum list
 
Laminating it with kevlar in some fashion might be (somewhat) effective. Maybe...

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Yeah, but it snags something awful :)

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Glue tire threads with steel belts to it. That is the material that gives me the most difficulty to cut. If anything, it will a lot of smoke and alert everyone in the area.
 
TugboatEng said:
Glue tire threads with steel belts to it. That is the material that gives me the most difficulty to cut. If anything, it will a lot of smoke and alert everyone in the area.

I can first-hand vouch for that...
and believe me, the pic doesn't do it justice.