Need to heat several braided rod assemblies at one one for application of solder.
 
Look in Industrial Heating magazine - there is a monthly section on induction heating with a recent one on coil design.
 
It is a good article.

We go to Ameritherm for this.

E. J. (Chip) LASKOWSKI
National Sales Manager
39 Main Street
Scottsville, New York 14546
Tel: 585-889-0246
Fax: 585-889-4030
chiplaskowski@ameritherm.com


Thomas J. Walz
Carbide Processors, Inc.
 
Thank you for the pointer to the magazine article, I'll check it out.
I looked at ameritherm's website, we are in the initial stages of testing the process. We have a decent machine now, just need to be able to process more than one at a time to get the cost down.
 
Amerithem is closed this week.

We do a lot of unusual carbide brazing. Last year we bought a couple of the little 1 kw Hot Shots systems from Ameritherm largely because of their tech support. (I have been doing brazing consulting for over twenty years and have seen a lot of folks with induction systems and no tech support.) Their lab is very good at designing solutions based on the parts we send them. The closest thing to a problem we have had is when we wanted to buy a couple new shapes for R&D. The salesperson didn’t want to sell them to until he was sure they would work. We just wanted to try a couple ideas and figured $1,000 for two coils wasn’t a whole lot. We contacted Girish Dahake (neat guy) directly and he had them made for us. They didn’t work very well in production but they did teach us a lot.

tom


Thomas J. Walz
Carbide Processors, Inc.
 