Attempting to replace a European mtrl specification with something commercially available in the USA. ASTM A514 has been suggested due to the fact that the required mechanical properties of ASTM A514 are within spec.
However, the original design required some sections to be induction hardened. Spec is HRC 50 0.3 mm deep, I know HRC is probably not applicable but this is the original spec on the drawing.
Can ASTM A514 safely and successfully induction hardened (without detriment to the core properties)?
It was my understanding that in general carbon content should be between 0.3-0.4% for induction hardening.
Thanks!
However, the original design required some sections to be induction hardened. Spec is HRC 50 0.3 mm deep, I know HRC is probably not applicable but this is the original spec on the drawing.
Can ASTM A514 safely and successfully induction hardened (without detriment to the core properties)?
It was my understanding that in general carbon content should be between 0.3-0.4% for induction hardening.
Thanks!