I have some hexagonal bar - appear to be cold drawn - hardness is around 400 BHN
Main elements determined on spectrometer
C 0.25%
Mn 1.65%
S 0.17%
no other elements at significant levels.

What is it?
 
Replies continue below

Recommended for you

Apart from trace levels of other elements the balance is iron.
 
HIGH MANGANESE CARBON STEEL simillar to SAE 1524 though S in your item is high.
 
Carburize;
Just curious, what is the specific application for the bar?
 
Its actually a failed piece from a very old farming implement. It was a drive shaft linking the PTO to a tiller.
 