Sep 28, 2004 #1 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US I have some hexagonal bar - appear to be cold drawn - hardness is around 400 BHN Main elements determined on spectrometer C 0.25% Mn 1.65% S 0.17% no other elements at significant levels. What is it?
I have some hexagonal bar - appear to be cold drawn - hardness is around 400 BHN Main elements determined on spectrometer C 0.25% Mn 1.65% S 0.17% no other elements at significant levels. What is it?
Sep 28, 2004 #2 IRstuff Aerospace Joined Jun 3, 2002 Messages 44,895 Location US What's the iron content? TTFN Upvote 0 Downvote
Sep 28, 2004 Thread starter #3 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US Apart from trace levels of other elements the balance is iron. Upvote 0 Downvote
Sep 28, 2004 #4 Rich2001 Mechanical Joined Mar 23, 2001 Messages 896 Location US HIGH MANGANESE CARBON STEEL simillar to SAE 1524 though S in your item is high. Upvote 0 Downvote
Sep 28, 2004 Thread starter #5 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US I think it is a re-sulfurized grade. Upvote 0 Downvote
Sep 28, 2004 #6 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Carburize; Just curious, what is the specific application for the bar? Upvote 0 Downvote
Sep 28, 2004 Thread starter #7 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US Its actually a failed piece from a very old farming implement. It was a drive shaft linking the PTO to a tiller. Upvote 0 Downvote
Its actually a failed piece from a very old farming implement. It was a drive shaft linking the PTO to a tiller.