ElCidCampeador
Mechanical
Hi there, I have a PQR for GTAW + GMAW processes, no impact test required.
In this PQR the minimum preheat temperature is set to 50°C.
Could I use it as support for a WPS GTAW+GMAW with minimum preheat temperature=100°C?
Increasing of min. preheat temperature appears in table QW-255/256 neither in essential nor supplemental variables. What does this mean? Does it mean that in the WPS I could increase this temperature whatever I want? thanks
In this PQR the minimum preheat temperature is set to 50°C.
Could I use it as support for a WPS GTAW+GMAW with minimum preheat temperature=100°C?
Increasing of min. preheat temperature appears in table QW-255/256 neither in essential nor supplemental variables. What does this mean? Does it mean that in the WPS I could increase this temperature whatever I want? thanks