Can anyone provide a value for the shear modulus of elasticity (modulus of rigidity) for inconel 600?
 
Go here:

Its a huge download but likely has that information inside.

(It is also my favorite metals reference book in the world! All that design data just waiting to be used... Thanks to whoever here turned me on to that one. And thanks to whoever wrote the dang thing.)

Nick
I love materials science!
 
I get a "no document found" response from this website. Any other way to access it?
 
boldfish- Hmm I tried that link and it worked for me....

Go to the main site:


Then enter the document ID:
MIL-HDBK-5J

And it should pull up the catalog you can download the PDF from. Its around 50MB or so.
 
Thanks, I found what I needed.
 