Dear All
What is the difference between INCONEL718 and INCONEL718PLUS manufacturing (lathe/milling)
(eg rpm/feed/depth/machining time), could we use the same parameter for 718 to work 718 plus,
thanks.
 
Joe Chen... Inconel [nickel alloy] 718 I am very familiar with... however Inconel718Plus is a term I am unfamiliar with... sounds like basic 718 with proprietary processing of some sort.

There are forums that might be more appropriate for this question...

Metals & metallurgy:
Machining:
BTW... when discussing alloys, be prepared to present the alloy material specification. IE: the specification that materials are 'made-per' are all-important in discussions like this.

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top