Good Morning All,
Kinda urgent issue. I had an N/S S-R test fail at 40+ hours in the notch for Inco 718 (AMS 5662/5663). Naturally we sent more material for the 3 redundant tests all of which broke in the notch in under 2 hours. I checked the solution H/T chart on our end and everything ran OK to the cycle and the lab was to perform the precipitation hardening then run the tests. On their end they say that the H/T ran smooth.
[ul]
[li]The specimens were taken from a thin walled forging in the longitudinal direction(0.5",~12.7mm)[/ul]
[/li]
[ul]
[li]I think that maybe the way specimen was machined in respect to the wall/surface defects may have been a factor.[/li]
[/ul]
Kinda urgent issue. I had an N/S S-R test fail at 40+ hours in the notch for Inco 718 (AMS 5662/5663). Naturally we sent more material for the 3 redundant tests all of which broke in the notch in under 2 hours. I checked the solution H/T chart on our end and everything ran OK to the cycle and the lab was to perform the precipitation hardening then run the tests. On their end they say that the H/T ran smooth.
[ul]
[li]The specimens were taken from a thin walled forging in the longitudinal direction(0.5",~12.7mm)[/ul]
[/li]
[ul]
[li]I think that maybe the way specimen was machined in respect to the wall/surface defects may have been a factor.[/li]
[/ul]