Jan 1, 2019 #1 feraidoon Materials Joined Feb 8, 2003 Messages 4 Location US thread330-330314 can any one help me for casting this alloy with low thermal expansion?
Jan 1, 2019 #2 arunmrao Materials Joined Oct 1, 2000 Messages 4,758 Location IN Provide more details of the part to be cast and quantities that you need. Also a literature review on the alloy characteristics will be helpful. "Even,if you are a minority of one, truth is the truth." Mahatma Gandhi. Upvote 0 Downvote