As per API 1104 APP B, in service welding is applicable for pipeline and piping system.
It means might be used to repair process piping as per ASME B31.3??
 
Not sure I get what you're asking, but yes, in service welding is commonly done on process piping with suitable engineering evaluation and proper precautions.

Nathan Brink
 
ASME PCC-2 would guide you to using API Std 1104 as an additional standard.

Steve Jones
Corrosion Management Consultant