Dario2002
Petroleum
- Aug 25, 2006
- 33
What are practical experiences with in service welding on high pressure gas pipeline (pressure containing metal sleeve)?
Assuming that welding procedure is verified, preheat is controlled (up to 100°C), surrounding temperature is quite low (around -5°C), natural gas is flowing through 20" pipe (GrX52, 7mm) at around 2-3 m/s, welding is inspected by ultrasound (B scan) and magnetoflux, is there any issues to be expected?
Is environment temperature of -5°C big influence in HAZ (heat affected zones), due to faster cooling, in comparison with possible spring/summer temperature of 20°C?
Assuming that welding procedure is verified, preheat is controlled (up to 100°C), surrounding temperature is quite low (around -5°C), natural gas is flowing through 20" pipe (GrX52, 7mm) at around 2-3 m/s, welding is inspected by ultrasound (B scan) and magnetoflux, is there any issues to be expected?
Is environment temperature of -5°C big influence in HAZ (heat affected zones), due to faster cooling, in comparison with possible spring/summer temperature of 20°C?