Has anybody had any experience with carrying out weld repairs to cracking on a 304H stainless steel vessel at 400 deg C. The vessel is not under pressure though operations are not keen to turn down the temperature to repair. Cracks are at a large nozzle to 300mm length. If anybody has had a similar experience welding at this temperature in any stainless some hints would be appreciated as to the feasibility, best welding method and what to watch for etc.
Thanks in advance
JonD71
JonD 71
Australia
Thanks in advance
JonD71
JonD 71
Australia