I'm looking for info on the wear characteristics of cast IN 100 on cast IN 100 at elevated temperatures, from 500°F to 1900°F. I'm hoping I won't have to apply a wear coating for a test that lasts under 500 hrs over the specified temperature ranges with low stresses, under 10,000 psi.
 
Replies continue below

Recommended for you

Contact your supplier of material. They may have done some basic friction and wear tests.

Alternativelky, you should consult published information on similar materials.

I think it is hard to find wear data for special materials, particularly for elevated temperature conditions.
 