hi friends
can anybody help me to solve this problem that i can not import this .inp file to abaqus?
the error is parametrized.i am trying to replace the real value, but the abaqus siad that :
WARNING: The following keywords/parameters are not yet supported by the input file reader:
---------------------------------------------------------------------------------
*CONTACTOUTPUT, MASTER, SLAVE"
please help me. the inp file is here:
*HEADING
3D Double cantilever beam test model
- use vcct *debond to model crack growth
orthogonal mesh, short run
**
**preprint,model=yes,history=yes,contact=yes
**Restart, Write
**
*parameter
** User input data defining the interface properties
** Fracture toughness (N/mm):
GIc = 1.2
GIIc = 6.0
GIIIc = 6.0
** B-K parameter:
eta = 1.75
modeMixLaw=3
** mixed mode parameter
am = 1.0
an=1.5
ao=1.0
** Damage and tolerance parameters
damv=0
**5.0e-5
tol=0.1
width=12.7
*NODE
1, 0.0, 0.0
11, 0.0, 1.0
51, 0.0, 0.0
61, 0.0, 1.0
**
**
9001, 4.5, 0.0
9011, 4.5, 1.0
9051, 4.5, 0.0
9061, 4.5, 1.0
**
18001, 9.0, 0.0
18011, 9.0, 1.0
18051, 9.0, 0.0
18061, 9.0, 1.0
**
*NGEN,NSET=NS1
1 , 9001, 100
51 , 9051, 100
9001 ,18001, 100
9051 ,18051, 100
*NGEN,NSET=NS2
11 , 9011, 100
61 , 9061, 100
9011 ,18011, 100
9061 ,18061, 100
**
*NFILL
NS1,NS2,10,1
**
**
*element,type=S4
20001, 1, 101, 102, 2
20051,51, 151, 152,52
**
*ELGEN,ELSET=lower_elements
20001, 180,100,100, 10, 1,1
*ELGEN,ELSET=upper_elements
20051, 180,100,100, 10, 1,1
**
**
*Shell Section, elset=upper_elements, material=MAT_upper,Orientation=Or1
0.2,
**
*Shell Section, elset=lower_elements, material=MAT_lower,Orientation=Or1
0.2,
**
*Orientation,Name=Or1
1.0, 0.0, 0.0, 0.0, 1.0, 0.0
3, 0.0
**
*MATERIAL,NAME=MAT_upper
*ELASTIC,TYPE=ENGINEERING CONSTANTS
8000000.0,8000000.0,8000000.0, 0.0, 0.0, 0.0,4000000.0,4000000.0,
4000000.0,
**
*MATERIAL,NAME=MAT_lower
*ELASTIC,TYPE=ENGINEERING CONSTANTS
8000000.0,8000000.0,8000000.0, 0.0, 0.0, 0.0,4000000.0,4000000.0,
4000000.0,
*elset,elset=slave,generate
20101,37901,100
20102,37902,100
20103,37903,100
20104,37904,100
20105,37905,100
20106,37906,100
20107,37907,100
20108,37908,100
20109,37909,100
20110,37910,100
*surface,type=element,name=slave
slave,SPOS
*surface,type=element,name=master
upper_elements,SNEG
*ELSET,ELSET=ETIED,GENERATE
29101,37901,100
29102,37902,100
29103,37903,100
29104,37904,100
29105,37905,100
29106,37906,100
29107,37907,100
29108,37908,100
29109,37909,100
29110,37910,100
*NSET,NSET=NTIED,ELSET=ETIED
*initial conditions, type=contact
slave, master,ntied
*Contact Pair, interaction=SURFS, small sliding, type=NODE TO SURFACE, no thickness
slave, master
*Surface Interaction, name=SURFS
1.,
*Friction, slip tolerance=0.005
0.,
*clearance,slave=slave,master=master,value=1.0E-8
*NSET,NSET=FIX,GENERATE
**18001, 18011
18051, 18061
*BOUNDARY
FIX,1,6
**
**
*MPC
BEAM, 1, 6
BEAM, 2, 6
BEAM, 3, 6
BEAM, 4, 6
BEAM, 5, 6
BEAM, 7, 6
BEAM, 8, 6
BEAM, 9, 6
BEAM,10, 6
BEAM,11, 6
**
BEAM, 51, 56
BEAM, 52, 56
BEAM, 53, 56
BEAM, 54, 56
BEAM, 55, 56
BEAM, 57, 56
BEAM, 58, 56
BEAM, 59, 56
BEAM, 60, 56
BEAM, 61, 56
**
**
*NSET, NSET=LP
6, 56
**
*************************************************************************************
**
**
** STEP: Step-1
**
** STEP: Step-1
**
*STEP, INC=1000
**,nlgeom
**
*STATIC,direct
0.107, 0.214
*debond, slave=slave, master=master
*FRACTURE CRITERION,TYPE=VCCT,MIXED MODE BEHAVIOR=REEDER,TOLERANCE=<tol>
<GIc>, <GIIc>, <GIIIc>, <eta>
*CONTROLS,PARAMETERS=TIME INCREMENTATION
, , , , , , , 10,
*BOUNDARY
**
6,3,3, -0.107
56,3,3, 0.107
**
**
**print,contact=yes
** OUTPUT REQUESTS
**
**Output, field, variable=PRESELECT
**Output, history, variable=PRESELECT
**NODE PRINT,NSET=LP
** U3, RF3
**
**
**output, field,freq=2
**node output
**u
**contact output,slave=slave,master=master
**sdv
*Output, history,freq=1
*NODE output,NSET=LP
U3, RF3
**energy output,var=all
*End Step
*STEP, INC=1000
**,nlgeom
**
*STATIC
**,stabilize=1.0E-8
0.001, 0.086,1.0E-8,0.002
**debond, slave=slave, master=master
**FRACTURE CRITERION,TYPE=VCCT,MIXED MODE BEHAVIOR=REEDER,TOLERANCE=<tol>
**<GIc>, <GIIc>, <GIIIc>, <eta>
*CONTROLS,PARAMETERS=TIME INCREMENTATION
, , , , , , , 10,
*BOUNDARY
**
6,3,3, -0.15
56,3,3, 0.15
**
**
**print,contact=yes
** OUTPUT REQUESTS
**
**Output, field, variable=PRESELECT
**Output, history, variable=PRESELECT
***NODE PRINT,NSET=LP
**U3, RF3
**
**
*output, field,freq=10
*element output
s
*node output
u
*contact output,slave=slave,master=master
dbt,dbsf,dbs,openbc,crsts,enrrt,efenrrtr,bdstat
*Output, history,freq=1
*NODE output,NSET=LP
U3, RF3
**energy output,var=all
*End Step
can anybody help me to solve this problem that i can not import this .inp file to abaqus?
the error is parametrized.i am trying to replace the real value, but the abaqus siad that :
WARNING: The following keywords/parameters are not yet supported by the input file reader:
---------------------------------------------------------------------------------
*CONTACTOUTPUT, MASTER, SLAVE"
please help me. the inp file is here:
*HEADING
3D Double cantilever beam test model
- use vcct *debond to model crack growth
orthogonal mesh, short run
**
**preprint,model=yes,history=yes,contact=yes
**Restart, Write
**
*parameter
** User input data defining the interface properties
** Fracture toughness (N/mm):
GIc = 1.2
GIIc = 6.0
GIIIc = 6.0
** B-K parameter:
eta = 1.75
modeMixLaw=3
** mixed mode parameter
am = 1.0
an=1.5
ao=1.0
** Damage and tolerance parameters
damv=0
**5.0e-5
tol=0.1
width=12.7
*NODE
1, 0.0, 0.0
11, 0.0, 1.0
51, 0.0, 0.0
61, 0.0, 1.0
**
**
9001, 4.5, 0.0
9011, 4.5, 1.0
9051, 4.5, 0.0
9061, 4.5, 1.0
**
18001, 9.0, 0.0
18011, 9.0, 1.0
18051, 9.0, 0.0
18061, 9.0, 1.0
**
*NGEN,NSET=NS1
1 , 9001, 100
51 , 9051, 100
9001 ,18001, 100
9051 ,18051, 100
*NGEN,NSET=NS2
11 , 9011, 100
61 , 9061, 100
9011 ,18011, 100
9061 ,18061, 100
**
*NFILL
NS1,NS2,10,1
**
**
*element,type=S4
20001, 1, 101, 102, 2
20051,51, 151, 152,52
**
*ELGEN,ELSET=lower_elements
20001, 180,100,100, 10, 1,1
*ELGEN,ELSET=upper_elements
20051, 180,100,100, 10, 1,1
**
**
*Shell Section, elset=upper_elements, material=MAT_upper,Orientation=Or1
0.2,
**
*Shell Section, elset=lower_elements, material=MAT_lower,Orientation=Or1
0.2,
**
*Orientation,Name=Or1
1.0, 0.0, 0.0, 0.0, 1.0, 0.0
3, 0.0
**
*MATERIAL,NAME=MAT_upper
*ELASTIC,TYPE=ENGINEERING CONSTANTS
8000000.0,8000000.0,8000000.0, 0.0, 0.0, 0.0,4000000.0,4000000.0,
4000000.0,
**
*MATERIAL,NAME=MAT_lower
*ELASTIC,TYPE=ENGINEERING CONSTANTS
8000000.0,8000000.0,8000000.0, 0.0, 0.0, 0.0,4000000.0,4000000.0,
4000000.0,
*elset,elset=slave,generate
20101,37901,100
20102,37902,100
20103,37903,100
20104,37904,100
20105,37905,100
20106,37906,100
20107,37907,100
20108,37908,100
20109,37909,100
20110,37910,100
*surface,type=element,name=slave
slave,SPOS
*surface,type=element,name=master
upper_elements,SNEG
*ELSET,ELSET=ETIED,GENERATE
29101,37901,100
29102,37902,100
29103,37903,100
29104,37904,100
29105,37905,100
29106,37906,100
29107,37907,100
29108,37908,100
29109,37909,100
29110,37910,100
*NSET,NSET=NTIED,ELSET=ETIED
*initial conditions, type=contact
slave, master,ntied
*Contact Pair, interaction=SURFS, small sliding, type=NODE TO SURFACE, no thickness
slave, master
*Surface Interaction, name=SURFS
1.,
*Friction, slip tolerance=0.005
0.,
*clearance,slave=slave,master=master,value=1.0E-8
*NSET,NSET=FIX,GENERATE
**18001, 18011
18051, 18061
*BOUNDARY
FIX,1,6
**
**
*MPC
BEAM, 1, 6
BEAM, 2, 6
BEAM, 3, 6
BEAM, 4, 6
BEAM, 5, 6
BEAM, 7, 6
BEAM, 8, 6
BEAM, 9, 6
BEAM,10, 6
BEAM,11, 6
**
BEAM, 51, 56
BEAM, 52, 56
BEAM, 53, 56
BEAM, 54, 56
BEAM, 55, 56
BEAM, 57, 56
BEAM, 58, 56
BEAM, 59, 56
BEAM, 60, 56
BEAM, 61, 56
**
**
*NSET, NSET=LP
6, 56
**
*************************************************************************************
**
**
** STEP: Step-1
**
** STEP: Step-1
**
*STEP, INC=1000
**,nlgeom
**
*STATIC,direct
0.107, 0.214
*debond, slave=slave, master=master
*FRACTURE CRITERION,TYPE=VCCT,MIXED MODE BEHAVIOR=REEDER,TOLERANCE=<tol>
<GIc>, <GIIc>, <GIIIc>, <eta>
*CONTROLS,PARAMETERS=TIME INCREMENTATION
, , , , , , , 10,
*BOUNDARY
**
6,3,3, -0.107
56,3,3, 0.107
**
**
**print,contact=yes
** OUTPUT REQUESTS
**
**Output, field, variable=PRESELECT
**Output, history, variable=PRESELECT
**NODE PRINT,NSET=LP
** U3, RF3
**
**
**output, field,freq=2
**node output
**u
**contact output,slave=slave,master=master
**sdv
*Output, history,freq=1
*NODE output,NSET=LP
U3, RF3
**energy output,var=all
*End Step
*STEP, INC=1000
**,nlgeom
**
*STATIC
**,stabilize=1.0E-8
0.001, 0.086,1.0E-8,0.002
**debond, slave=slave, master=master
**FRACTURE CRITERION,TYPE=VCCT,MIXED MODE BEHAVIOR=REEDER,TOLERANCE=<tol>
**<GIc>, <GIIc>, <GIIIc>, <eta>
*CONTROLS,PARAMETERS=TIME INCREMENTATION
, , , , , , , 10,
*BOUNDARY
**
6,3,3, -0.15
56,3,3, 0.15
**
**
**print,contact=yes
** OUTPUT REQUESTS
**
**Output, field, variable=PRESELECT
**Output, history, variable=PRESELECT
***NODE PRINT,NSET=LP
**U3, RF3
**
**
*output, field,freq=10
*element output
s
*node output
u
*contact output,slave=slave,master=master
dbt,dbsf,dbs,openbc,crsts,enrrt,efenrrtr,bdstat
*Output, history,freq=1
*NODE output,NSET=LP
U3, RF3
**energy output,var=all
*End Step