I have a question on the welding procedure . ASME IX is used for the welding procedure qualification but Supervised project under b31.3. Impact testing is required.
PQR: GTAW + SMAW;
Test coupon thickness: 23.83mm;
Deposited welds thickness: GTAW: 5.0mm; SMAW: 18.83
now: we need welding ONLY with GTAW.
I can use this PQR to support a WPS with impact testing, just for gtaw.
Thanks for your help.