Hello Fellow Engineers,
We are currently fabricating some pressure vessels for a project, which follows SHELL DEP & the vessel design code is ASME section VIII- Div 1.
Our MDMT is about -6 DEG C. Max thickness for pressure parts is 15 mm.(varying from 6 mm to 15 mm)
A cl. in the SHELL DEP for unfired pressure vessels states the following
"Impact Testing and Impact values shall comply as per the code of construction. Exemptions to impact testing or a change in impact test temperature if permitted by the code shall not be permitted."
Does the above mean that irrespective of the thickness we need to impact test the material for pressure parts?
We are currently fabricating some pressure vessels for a project, which follows SHELL DEP & the vessel design code is ASME section VIII- Div 1.
Our MDMT is about -6 DEG C. Max thickness for pressure parts is 15 mm.(varying from 6 mm to 15 mm)
A cl. in the SHELL DEP for unfired pressure vessels states the following
"Impact Testing and Impact values shall comply as per the code of construction. Exemptions to impact testing or a change in impact test temperature if permitted by the code shall not be permitted."
Does the above mean that irrespective of the thickness we need to impact test the material for pressure parts?