hello friends
i am using my impact test welding procedure for 3/4" shell thickness do i have to still need production run off plates for
cat A & cat B. & do i need ferrite content examination on my weld procedure.
please advice.
stanly
 
Replies continue below

Recommended for you

More information and more clarity is required in the questions.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 