Hi All
The design temperature is for our project is -68 degree C.The material selected is ASTM A333 Gr.6.As per my understanding impact test temperature for ASTM A 333 gr.6 is -45 degree C.Please clarify whether impact test can be done at -70 degree Celsius for ASTM A 333 Gr.6 material.