Construction code ASME B31.3
Material A106 Gr. B
The thickness of Pipe. 17.48 mm
Temperature Limit 0^ F (-17.78^ C)
PWHT yes.
Table A-1 refers to curve B
Table 323.2.2A minimum Temperature without Impact Testing for CS showing under curve B 9^ F ( 12.8^ C).
My Question is for above case Impact testing for WPS qualification is required?
 
I suppose the answer is in your own question.
 
Get a relevant PQR thar has inpact test in it. Make a WPS using this PQR.

DHURJATI SEN
Kolkata, India


 