hi every body
i need to know that astm a105 flange if normalized, belongs to which curve in asme b31.3, Fig. 323.2.2A Minimum Temperatures Without Impact Testing for Carbon Steel Materials????
in table a-1 materials with heat treatment are not listed, like this material. please help me to explain for my client for minimum design temperature of this material...
 
Per Table A-1, the Min Temp for A105 without impact testing is -20°F.

Normalizing doesn't get you any lower temperature.
 
thnks for your answer but please refer me to standards and codes to proof your answer
 
My proof is that ASME B31.3 does not provide any rules to allow a reduction of the minimum temperature for normalized A105 material below -20°F. Please review ASME B31.3 for your own understanding.
 
Ok. Thnks. But i am not satisfied![ponder]
 
In ucs-66 also there is not any helpful information!
Please help me....
Our inspector will satisfy only with text in asme b31.3 or asme sec8 div1!
 
See 323.2.2(a)
Then see Table A-1 for A105 material. See Note 6 which is referenced in the 'Min. Temp.' heading of Table A-1.
 
Minimum temperature without impact testing does not necessarily equate to minimum design temperature.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
THANK YOU ALL...WITH THESE ANSWERS, NOW I HAVE A BETTER PERCEPTION ON THIS SUBJECT.....
I FINALLY DECIDE TO DO IMPACT TEST ON THIS PART.....