Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Impact Test Reduction

Status
Not open for further replies.

loilfan

Mechanical
Jan 20, 2015
122
We have a low temp vessel where the MDMT was determined by impact testing (i.e. was not exempted in Figure UCS-66) to -50F. If we want to reduce the MDMT to a lower temperature (say -60F), are we able to use the reduction from the stress ratio in Figure UCS-66.1 without doing any further impact tests?

My thought is that this would be acceptable since the -50F impact test assumed a fully loaded material.
 
Replies continue below

Recommended for you

Take a look into UCS-66(i), this may be of help for you. However I believe that by doing so that would be considered as an alteration on exisitng vessel.

Regards.
 
Thanks Jano6924, that's the reference I needed. And you are correct that this would absolutely be an alteration, albeit a non-physical change.
 
Yes, this is an alteration as a re-rating and would be under either rules from the NBIC Part 3 or API 510.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor