I am qualifying a test coupon Sa333 Gr 6 to Sa 350 LF2. I have to carry out impact test at -50°F. The location of the specimen for impacts will be as follows
Set "A"
weld center Line
Haz on the pipe side
Haz on the flange side
PM on the Pipe side
PM on the Flange side
Set "B"
weld center Line
Haz on the pipe side
Haz on the flange side
PM on the Pipe side
PM on the Flange side
Set "C"
weld center Line
Haz on the pipe side
Haz on the flange side
PM on the Pipe side
PM on the Flange side
Can someone tell me whether I am doing the right thing
Regards
Merzi
Set "A"
weld center Line
Haz on the pipe side
Haz on the flange side
PM on the Pipe side
PM on the Flange side
Set "B"
weld center Line
Haz on the pipe side
Haz on the flange side
PM on the Pipe side
PM on the Flange side
Set "C"
weld center Line
Haz on the pipe side
Haz on the flange side
PM on the Pipe side
PM on the Flange side
Can someone tell me whether I am doing the right thing
Regards
Merzi