Hi Engineers,

I am having the following pipe material and size:

Material: SA 106 B pipe
Size: 1.5 inch SCH 40 (3.68 mm thickness)

And I have to comply to PED impact test requirement.


Question: Is it possible to do impact test on 3.68mm thk?

Thank you!
 
Replies continue below

Recommended for you

ASTM A370 describes subsize specimens. Two of the sizes described by this spec are 10mm X 2.5mm X 55mm and 10mm X 3.3mm X 55mm.

What does your customer say?

Engineering is not the science behind building. It is the science behind not building.
 
You might also check with your testing lab to see if they have any problems with thin material.
 
Dear all,

Thanks for the replies. Maybe let me elaborate further on my questions.

Basically we are trying to fulfill the requirement as per Section 7.5, Annex I, PED where its bending rupture energy measured on an ISO V test-piece is no less than 27 J, at a temperature not greater than 20 °C but not higher than the lowest scheduled operating temperature.

As mentioned, our pipe size is 1.5 inch SCH 40 (3.68 mm thickness), which the thickness is less than reference specimen thickness of 10 mm. I read that when a test piece of 10 mm x 10 mm cannot be obtained, it is necessary to use a sub-sized specimen of at least of 5 mm thickness and to adjust the value of impact test (based on EN 13445-2, the adjusted value is 14 J). And for test piece with thickness less than 5 mm, the verification of the specified 27 J is not required.

And according to ISO 148-1, the smallest sub-size can be defined in 10 mm X 2.5 mm X 55 mm.

So the question is, is it possible and necessary to do impact test on 1.5 inch SCH 40 pipe with thickness less than 5 mm? If yes, what is the value of impact test that I should refer in order to comply to PED?
 