Dear Members
In one of the pressure vessel,designed as per ASME SEC VIII
the raw material SA 516 gr 70 ( 3 in thk)which is being used from existing stock,is impact tested at minus 30 deg F and the impact values are satisfactory ( 100J)
The vessel is to be post weld heat treated. As per CLIENT specification requirements ,the raw material is to be impact tested at minus 50 deg F after Simulated PWHT .
I would like to know that if after simulated PWHT will their will be any change in impact properties ?For Ex If the raw material say is impact tested at minus 50 F, what will be the effect of SPWHT on impact properties ?
Secondly will the no of cycles of PWHT ( second/third)will have any effect on impact properties?
Any useful links on this subject will be appreciated
Thanks in advance
Sridhar
In one of the pressure vessel,designed as per ASME SEC VIII
the raw material SA 516 gr 70 ( 3 in thk)which is being used from existing stock,is impact tested at minus 30 deg F and the impact values are satisfactory ( 100J)
The vessel is to be post weld heat treated. As per CLIENT specification requirements ,the raw material is to be impact tested at minus 50 deg F after Simulated PWHT .
I would like to know that if after simulated PWHT will their will be any change in impact properties ?For Ex If the raw material say is impact tested at minus 50 F, what will be the effect of SPWHT on impact properties ?
Secondly will the no of cycles of PWHT ( second/third)will have any effect on impact properties?
Any useful links on this subject will be appreciated
Thanks in advance
Sridhar