hi
could some body introduce me for performing one trainning course
for weldoverlaying clad with alloy 625 to do this course in iran.
regards,
Reza Salimi
r_salimi@boushehr.sadragroup.com
 
Replies continue below

Recommended for you

See
I just finished a 625 job for FMC in Brazil, overlay and SMAW on 8630 material. Qualified PQR's/WPS's.

Two day course would be offered.

Regards,
Steve Snyder
 