I have a titanium part that is glass bead peaned prior to passivation. The bead blast media is also used on 300, 400 series stainless steels as well as 14-4 PH and MP35N materials.
Will the passivation remove any imbedded particles in the titanium from the other materials or is there still a chance for cross contamination?
Will the passivation remove any imbedded particles in the titanium from the other materials or is there still a chance for cross contamination?