NKBeresford
Petroleum
I have an Alloy 825 pipe system -
DT= 654°F; DP = 2820psig.
TP = 1.5*(2820)*(23.3/17.484) rounded up to next 25 psig increment or 5650 psig.
ASME B16.5 Class 1500 flange rating @ 100°F equals 3750psig. (Table F2-3.8)
Per Para 2.6 - I can system test these flanges to 1.5*3750 = 5625psig.
B31.3 Para 345.4.2 (c) states that the TP cannot produce a nominal pressure stress or longitudinal stress in excess of the yield strength at test temp.
How do I determine this?
What is my test pressure for this line?
DT= 654°F; DP = 2820psig.
TP = 1.5*(2820)*(23.3/17.484) rounded up to next 25 psig increment or 5650 psig.
ASME B16.5 Class 1500 flange rating @ 100°F equals 3750psig. (Table F2-3.8)
Per Para 2.6 - I can system test these flanges to 1.5*3750 = 5625psig.
B31.3 Para 345.4.2 (c) states that the TP cannot produce a nominal pressure stress or longitudinal stress in excess of the yield strength at test temp.
How do I determine this?
What is my test pressure for this line?