Jul 5, 2005 #1 aniiie Materials Joined Jul 5, 2005 Messages 5 Location DE Hi, we are just starting with trials on hybrid laser/MAG welding of X70. The laser power,12kW, the material thickness 12.7mm. Does enyone have some usefull experiences or information about the process parameters and settings? Thanks in advance...
Hi, we are just starting with trials on hybrid laser/MAG welding of X70. The laser power,12kW, the material thickness 12.7mm. Does enyone have some usefull experiences or information about the process parameters and settings? Thanks in advance...