Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

HWS Weld Callout

Status
Not open for further replies.

Revv

Structural
Aug 23, 2021
87
Hey Guys,

What weld callout do you usually show for your headed weld studs to embed plate?

Thank you!
 
Replies continue below

Recommended for you

I usually dont.
Isn't this an industry standard thing where the weld is sufficient to develop the strength of the stud?
 
AWS D1.1 has specific requirements for stud welding, I believe. It's either done using a weld gun that actually fuses the base of the stud onto the base metal, or there's an alternate allowance for a fillet weld. Personally, if it's small quantity where I'm not confident that the shop will understand the work, I'll sometimes just call out that I want it performed as a full fusion stud weld as per AWS D1.1 and then call out a fillet weld alternate with a size right on the drawing. That size will be enough to develop the stud. Then if they're inexperience in that type of work or don't have a qualified procedure they'll just go ahead and do the fillet.
 