Mar 12, 2009 #1 vendo Mechanical Joined Nov 13, 2007 Messages 2 Location US I can not find the thickness tolerance to apply to HR Steel at .250
Mar 12, 2009 #2 Bribyk Mechanical Joined Aug 14, 2007 Messages 440 Location CA Try here: http://www.russelmetals.com/pdf/english/service/pdf_catalogue/Sec_04_Steel_Plates.pdf Upvote 0 Downvote
Mar 13, 2009 #3 ajh1 Structural Joined Mar 8, 2002 Messages 448 Location US ASTM practice for plates (material 0.235" and thicker) is -0.01" / + 0.03" to 0.04" depending on width of plate. ASTM A6 Table 1. Upvote 0 Downvote
ASTM practice for plates (material 0.235" and thicker) is -0.01" / + 0.03" to 0.04" depending on width of plate. ASTM A6 Table 1.
Mar 16, 2009 #4 JayCarp Mechanical Joined Aug 16, 2006 Messages 12 Location US I might add that for pressure vessel use the thickness MAY go .010 undersize with no penalties - Upvote 0 Downvote