rufi4212

Materials
Joined
Feb 23, 2011
Messages
1
Location
IN
Issue - During the pre-commissioning phase, the commissioning team discovered an issue with a 12-inch two-pipe weld, specifically that both pipe seams were continuously welded and the line has successfully hydrostatic testing has passed, and non-destructive testing (NDT) has successfully done.
 
So what is the issue if its passed hydro and NDT??

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
IMO, for the piping construction, any pipe weld needs to be repaired prior to hydrotest if there is a NDT issue of the weld.
 
Does this 12" diameter pipe have 2 weld seams? If so how can it be continuous welded?
 
I wonder if the issue is the two x longitudinal seams are aligned and not off-set ?
 
DekDee, I suspect that is the issue.

AFAIK, this isn't a requirement in B31.3 just usually in a construction spec.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
You mean welds are not offset on ow different joints? There is still a girth weld in between them, they are not continuous... Not a big issue.
 