andradesilva
Materials
hi,
I am simulating blow-moulding of a parison to a bottle in ANSYS Polyflow. The problem is that the parison should stop inflating
upon contact with the mould, and the parison either inflates beyond the limits of the mould or it deforms in a very strange
way upon contact with the mould, depending if I deactivate mould release, or if I active it (I input a force adesion density value=1e6 N)
how can I put the parison to "glue" to the mould upon contact?
Any help appreciated,
Best regards,
I am simulating blow-moulding of a parison to a bottle in ANSYS Polyflow. The problem is that the parison should stop inflating
upon contact with the mould, and the parison either inflates beyond the limits of the mould or it deforms in a very strange
way upon contact with the mould, depending if I deactivate mould release, or if I active it (I input a force adesion density value=1e6 N)
how can I put the parison to "glue" to the mould upon contact?
Any help appreciated,
Best regards,