The aluminum part i want to protect is part of a washing machine. It's called a spider-arm, and it's attached to a stainless steel drum. The drum is of course where you put your clothes. It spins at speeds of 1200rpm. The load (clothes) can be unevenly distributed in the drum, therefore it could be put through high stress. This setup is (afaik) only on front load washers.
The thing is, the spider always corrodes and breaks - mine did in just 3 years. It's inevitable. Lots of theories as to why that happens...galvanic corrosion, water PH levels, too little detergent, too much detergent, using cold water, keeping the washer door closed, not using bleach...and so on.
Those who say it's NOT galvanic corrosion argue that if it was, the spider would have corroded at the points where it meets the stainless steel drum (the 3 ends), and at the shaft. Although most of the corroded spiders i've seen corrode a few inches up the shaft, i'm yet to see most of the corrosion happening at the spider-arm end joints...or immediately at the shaft. So they are of the opinion that the reason it is corroding is because of soap and high PH water.
In any case, i am getting ready to put in a new spider-arm and i would like to treat/coat it (and/or the stainless steel directly under it) so that i could get at least 10 years out of it. What would be the best method?
Greatly appreciate any help i can get!
Click here for more pics (Google image)

The thing is, the spider always corrodes and breaks - mine did in just 3 years. It's inevitable. Lots of theories as to why that happens...galvanic corrosion, water PH levels, too little detergent, too much detergent, using cold water, keeping the washer door closed, not using bleach...and so on.
Those who say it's NOT galvanic corrosion argue that if it was, the spider would have corroded at the points where it meets the stainless steel drum (the 3 ends), and at the shaft. Although most of the corroded spiders i've seen corrode a few inches up the shaft, i'm yet to see most of the corrosion happening at the spider-arm end joints...or immediately at the shaft. So they are of the opinion that the reason it is corroding is because of soap and high PH water.
In any case, i am getting ready to put in a new spider-arm and i would like to treat/coat it (and/or the stainless steel directly under it) so that i could get at least 10 years out of it. What would be the best method?
Greatly appreciate any help i can get!