Oct 8, 2019 #1 jtseng123 Mechanical Joined Jun 6, 2012 Messages 530 Location US Dear all, Can anyone provide some guidelines how to prevent sigma phase embrittlement on welds for 304H SS. This is for part in 1450 degF design temperature.
Dear all, Can anyone provide some guidelines how to prevent sigma phase embrittlement on welds for 304H SS. This is for part in 1450 degF design temperature.
Oct 8, 2019 #2 XL83NL Mechanical Joined Mar 3, 2011 Messages 3,120 Location NL [ol 1] [li]API RP 571 (2011), section 4, para 4.2.6. Prevention/mititgation is detailed in 4.2.6.6[/li] [li]WRC 489 (2004), section 4, para 4.2.6 (essentially the same as 1. above).[/li] [/ol] Upvote 0 Downvote
[ol 1] [li]API RP 571 (2011), section 4, para 4.2.6. Prevention/mititgation is detailed in 4.2.6.6[/li] [li]WRC 489 (2004), section 4, para 4.2.6 (essentially the same as 1. above).[/li] [/ol]