Dear all,

Can anyone provide some guidelines how to prevent sigma phase embrittlement on welds for 304H SS.

This is for part in 1450 degF design temperature.
 
Replies continue below

Recommended for you

[ol 1]
[li]API RP 571 (2011), section 4, para 4.2.6. Prevention/mititgation is detailed in 4.2.6.6[/li]
[li]WRC 489 (2004), section 4, para 4.2.6 (essentially the same as 1. above).[/li]