Hi guys,

I have been trying to polish titanium64 without reaching the final stage(0.04 microns) as I don't want the sample partially polished but, I always have scratches on which I cannot afford.

Anyone with experience in preparation of titanium samples??
 
Replies continue below

Recommended for you

Try using "clean" abrasive pads, nothing that has been used on anything else. Burrs can be embedded in the larger grits (ie 400-800) that will tear your specimen up with scratches that will be too deep for finer grits to get out. if you get a deep scratch, go back to square 1 and start over.
 