Dec 14, 2015 #1 fahimahammad Civil/Environmental Joined Nov 10, 2015 Messages 6 Location US ASTM does not say any thing about mold size or how to fill mold. What is the mold size ? And how to fill mold with sample (any compection needed?) Plz tell me.
ASTM does not say any thing about mold size or how to fill mold. What is the mold size ? And how to fill mold with sample (any compection needed?) Plz tell me.
Dec 22, 2015 #2 D27 Civil/Environmental Joined Nov 19, 2015 Messages 8 Location SB are you asking for concrete sampling? if yes its ASTM C31 Upvote 0 Downvote
Dec 23, 2015 Thread starter #3 fahimahammad Civil/Environmental Joined Nov 10, 2015 Messages 6 Location US No , its for laboratory vane shear test of clay soil. Upvote 0 Downvote