lganga
Mechanical
- Apr 10, 2011
- 109
The Vessel is a 70’ x 10´ double wall reactor. Inner Shell is a 30 mm thickness wall CS with 316L 3 mm clad.
Outer shell is a CS and it contains the cooling or heating water, depending of the stage of the inner vessel reaction.
We want to check the thickness of the inner wall with clad steel but the only way to do it is from the inside of the vessel.
As we do not have any Ultrasonic thickness device that measure the clad and the CS from the clad side of the vessel (inside inner shell).
Question: Have anyone of you found this kind of problem before?. How did you solve it?