Hi there.
I'm currently dealing with an magnetic issue in one of my 700 plastic injection molds.
It's a huge mold (arroud 1 cubic meter volume).
Can you give me a "simple" and economically interesting way to release that amount of steel from magnetic forces?...it's getting difficult to deal with all the magnetic sensores inside it to manage the movement of the parts. They became very unstable and security has been compromised.
The is always the change to unmount the mold into pieces, although the 1mx1m section is always present in the plates of the mold.
Thanks.
Best regards
RDias
I'm currently dealing with an magnetic issue in one of my 700 plastic injection molds.
It's a huge mold (arroud 1 cubic meter volume).
Can you give me a "simple" and economically interesting way to release that amount of steel from magnetic forces?...it's getting difficult to deal with all the magnetic sensores inside it to manage the movement of the parts. They became very unstable and security has been compromised.
The is always the change to unmount the mold into pieces, although the 1mx1m section is always present in the plates of the mold.
Thanks.
Best regards
RDias